分类 温度 | 产品|项目 | 比重 g/cm3 | 重烧线变化% | 冷态耐 压强度 MPa | 热膨胀 (1000℃) % | 导热系数 (350℃) W/m.K |
1260 | JSJM | 0.55 | ( | 1.1 | 0.5 | 0.16 |
1260 | JSJM -23B | 0.8 | | 2.0 | 0.5 | 0.24 |
1400 | JSJM | 0.8 | ( | 2.4 | 0.5 | 0.25 |
1400 | JSJM -26B | 0.8 | ( | 2.4 | 0.5 | 0.25 |
1500 | JSJM | 0.8 | ( | 2.8 | 0.55 | 0.28 |
1500 | JSJM -28B | 0.9 | ( | 3.3 | 0.55 | 0.33 |
1550 | JSJM | 0.9 | ( | 3.5 | 0.58 | 0.35 |
1550 | JSJM -30B | 1.0 | ( | 4.0 | 0.58 | 0.39 |
1600 | JSJM | 1.0 | ( | 4.5 | 0.6 | 0.40 |
1600 | JSJM -32B | 1.1 | ( | 4.8 | 0.6 | 0.43 |